Chemical Composition
0.17
%  (maximum)  
0.4 to 0.7
%    
0.3 to 0.5
%    
96.3 to 98.5
%    (estimate)
0.5 to 1.2
%    
0.1
%  (maximum)  
0.005 to 0.05
%    
0.4
%  (maximum)  
0.04
%  (maximum)  
0.05
%  (maximum)  
0.25 to 0.5
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
345
MPa  (minimum)  
485
MPa  (minimum)  
21
% strain  (minimum)  
 
Other Information