Chemical Composition
0.001 to 0.005
%    
0.1 to 0.2
%    
97.4 to 98.2
%    (estimate)
1.1 to 1.5
%    
0.45 to 0.55
%    
0.035
%  (maximum)  
0.035
%  (maximum)  
0.15 to 0.3
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
690
MPa  (minimum)  
760 to 895
MPa    
18
% strain  (minimum)  
 
Other Information
Links