Chemical Composition
0.23
%  (maximum)  
1.5 to 2
%    
92.4 to 95.2
%    (estimate)
0.2 to 0.4
%    
0.4 to 0.6
%    
2.75 to 3.9
%    
0.02
%  (maximum)  
0.02
%  (maximum)  
0.4
%  (maximum)  
0.03
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
490
MPa  (minimum)  
620 to 795
MPa    
18
% strain  (minimum)  
 
Other Information