Chemical Composition
0.05
%  (maximum)  
0.3
%  (maximum)  
0.4
%  (maximum)  
0.35
%  (maximum)  
96.5 to 99.3
%    (estimate)
0.6 to 1.35
%    
0.1
%  (maximum)  
0.5
%  (maximum)  
0.02
%  (maximum)  
0.02
%  (maximum)  
0.15 to 0.35
%    
0.05
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
205
MPa  (minimum)  
415 to 585
MPa    
25
% strain  (minimum)  
 
Other Information
Links



No warranty is given for the accuracy of these data