Layout: No layout
View
Summary datasheet
Printable datasheet
Show empty items
Record properties
Expand headings
Collapse headings
Expand all metadata
Collapse all metadata
Change layout
No layout
~Release Layout
Alloy Finder (Default)
Explore Chemical Composition
Explore Properties
Tools
Add to list
Copy to clipboard
Export to text file…
Export to Excel…
Find substitutes for this record
View related records
Watch data…
Watch this record
Bookmark
Units
Metric
CGS (Consistent)
FPS (Consistent)
IPS (Consistent)
SI (Consistent)
UK Imperial
US Customary
Boron steel, Grade H, ASTM A517/A517M-93
add data link
Range attributes
B (Boron)
0.0005
% (minimum)
C (Carbon)
0.12 to 0.21
%
Cr (Chromium)
0.4 to 0.65
%
Elongation
16
% strain (minimum)
Fe (Iron)
96.3 to 97.8
%
(estimate)
Mn (Manganese)
0.95 to 1.3
%
Mo (Molybdenum)
0.2 to 0.3
%
Ni (Nickel)
0.3 to 0.7
%
P (Phosphorus)
0.035
% (maximum)
S (Sulfur)
0.035
% (maximum)
Si (Silicon)
0.15 to 0.35
%
Ultimate Tensile Strength
795 to 930
MPa
V (Vanadium)
0.03 to 0.08
%
Yield Strength
690
MPa (minimum)
Discrete attributes
~Checking Status
Not verified - Original build
Date Last Checked
Thursday, October 17, 2013
Alloy Family
Alloy Steel
Alloy Group
Miscellaneous or unclassified
Alloy Sub-Group
Boron steel
Available forms
Wrought
Base Element
Fe (Iron)
Country
USA
Material Class
Ferrous Alloy
Source
Worldwide Guide to Equivalent Irons and Steels, 5th ed. ASM International 2006
Specification Status
Active
Specification Type
Standard
Standards Body
ASTM (USA)
Short text attributes
Composition Note_old
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Country*
USA
Description_old
High-strength alloy steel plates for use in fusion welded boilers and other pressure vessels; QT, t<=50 mm.
Designation
Grade H
Specification
ASTM A517/A517M-93
Specification Status Notes
active 2004
Long text attributes
Composition Note
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Description
High-strength alloy steel plates for use in fusion welded boilers and other pressure vessels; QT, t<=50 mm.
Hyperlink attributes
Similar Alloys
Click here to find similar alloys
Integer attributes
Specification Year
2004
Further Information
Organizations
American Society for Testing and Materials (ASTM)
No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®
UNHANDLED ERROR!
View log for stack trace
Close
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch record
Add to list
Copy to clipboard
Watch folder
Download Excel Template
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch generic
Download Excel Template
Add to list
Copy to clipboard
Watch table
Download Excel Template
Add all results from this table to list
Copy all results from this table to clipboard
Watch table
Add to list
Copy to clipboard
Find substitutes for this record
Watch record
Add all to list
Copy all to clipboard
Add all to list
Copy all to clipboard