Chemical Composition
0.02 to 0.08
%    
0.31
%  (maximum)  
0.3
%  (maximum)  
0.4
%  (maximum)  
96.9 to 100
%    (estimate)
1.35
%  (maximum)  
0.12
%  (maximum)  
0.02
%  (maximum)  
0.4
%  (maximum)  
0.035
%  (maximum)  
0.035
%  (maximum)  
0.03
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
310
MPa  (minimum)  
515 to 655
MPa    
13 to 16
% strain    
 
Other Information
Links



No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®