Chemical Composition
0.001 to 0.003
%    
0.05 to 0.15
%    
2.7 to 3.3
%    
94.4 to 95.8
%    (estimate)
0.3 to 0.6
%    
0.9 to 1.1
%    
0.02
%  (maximum)  
0.02
%  (maximum)  
0.1
%  (maximum)  
0.015 to 0.035
%    
0.2 to 0.3
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
415
MPa  (minimum)  
585 to 760
MPa    
18
% strain  (minimum)  
 