Chemical Composition
0.05 to 0.15
%    
2 to 2.5
%    
95.1 to 96.8
%    (estimate)
0.3 to 0.6
%    
0.9 to 1.1
%    
0.025
%  (maximum)  
0.025
%  (maximum)  
0.5
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
205
MPa  (minimum)  
415 to 585
MPa    
20
% strain  (minimum)  
 
Other Information
Links



No warranty is given for the accuracy of these data