Chemical Composition
0.1 to 0.2
%    
1 to 1.5
%    
95.8 to 97.7
%    (estimate)
0.3 to 0.8
%    
0.45 to 0.65
%    
0.025
%  (maximum)  
0.025
%  (maximum)  
0.5 to 1
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
310
MPa  (minimum)  
515 to 690
MPa    
18
% strain  (minimum)  
 
Other Information