Chemical Composition
0.25 to 0.35
%    
0.8 to 1.15
%    
97 to 98.2
%    (estimate)
0.4 to 0.9
%    
0.15 to 0.25
%    
0.025
%  (maximum)  
0.025
%  (maximum)  
0.15 to 0.35
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
485
MPa  (minimum)  
825 to 1000
MPa    
18
% strain  (minimum)  
248
 (minimum)  
 
Other Information
Links



No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®