Chemical Composition
0.4 to 0.55
%    
98.5 to 98.9
%    (estimate)
0.6 to 0.9
%    
0.045
%  (maximum)  
0.05
%  (maximum)  
0.15
%  (minimum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
295
MPa  (minimum)  
570
MPa  (minimum)  
23
% strain  (minimum)  
 
Other Information