Chemical Composition
0.0005 to 0.002
%    
0.09
%  (maximum)  
0.3
%  (maximum)  
0.5
%  (maximum)  
91.3 to 97.9
%    (estimate)
1 to 2
%    
0.4
%  (maximum)  
0.05
%  (maximum)  
1 to 5
%    
0.01
%  (maximum)  
0.005
%  (maximum)  
0.05 to 0.25
%    
0.006 to 0.03
%    
0.02
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
690
MPa  (minimum)  
1000 to 1170
MPa    
13
% strain  (minimum)  
 
Other Information
Links