Chemical Composition
0.17 to 0.22
%    
0.25
%  (maximum)  
0.35
%  (maximum)  
95.8 to 97.4
%    (estimate)
0.45 to 0.65
%    
0.2 to 0.3
%    
1.65 to 2
%    
0.035
%  (maximum)  
0.04
%  (maximum)  
0.15 to 0.35
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
229
 (maximum)  
 
Other Information