Chemical Composition
0.02
%  (minimum)  
0.16
%  (maximum)  
0.2
%  (maximum)  
0.2
%  (maximum)  
96.3 to 100
%    (estimate)
1.6
%  (maximum)  
0.08
%  (maximum)  
0.015
%  (minimum)  
0.04
%  (maximum)  
0.2
%  (maximum)  
0.025
%  (maximum)  
0.025
%  (maximum)  
0.5
%  (maximum)  
0.05
%  (maximum)  
0.6
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Other Information