Chemical Composition
0.015
%  (minimum)  
0.005
%  (maximum)  
0.12
%  (maximum)  
96.4 to 100
%    (estimate)
1.9
%  (maximum)  
0.5
%  (maximum)  
0.09
%  (maximum)  
0.025
%  (maximum)  
0.015
%  (maximum)  
0.5
%  (maximum)  
0.22
%  (maximum)  
0.2
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
600
MPa  (minimum)  
650
MPa  (minimum)  
13
% strain  (minimum)  
 