Chemical Composition
0.22
%  (maximum)  
97.5 to 100
%    (estimate)
1.6
%  (maximum)  
0.04
%  (maximum)  
0.04
%  (maximum)  
0.55
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
355
MPa    
510 to 680
MPa    
12 to 14
% strain    
 
Other Information