Chemical Composition
0.02 to 0.1
%    
0.2
%  (maximum)  
96.9 to 100
%    (estimate)
2
%  (maximum)  
0.07
%  (maximum)  
0.045
%  (maximum)  
0.045
%  (maximum)  
0.6
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
Not Applicable
32.6
ksi    
49.3 to 68.2
ksi    
24 to 26
% strain    
 
Other Information