Chemical Composition
2.6
%  (maximum)  
0.2
%  (maximum)  
0.5
%  (maximum)  
65.7 to 72.5
%    (estimate)
4 to 4.5
%    
22 to 24
%    
1.5 to 2.5
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
210
MPa  (minimum)  
440
MPa  (minimum)  
25
% strain  (minimum)  
 
Other Information
Links



No warranty is given for the accuracy of these data