Chemical Composition
0.5 to 0.6
%    
19.3 to 21.5
%    
64.4 to 71.5
%    (estimate)
7 to 10
%    
0.2 to 0.4
%    
1.5 to 2.75
%    
0.05
%  (maximum)  
0.03
%  (maximum)  
0.25
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
700
MPa    
1080
MPa    
 
Other Information
Links



No warranty is given for the accuracy of these data