Chemical Composition
0.1
%  (maximum)  
0.12
%  (maximum)  
0.3
%  (maximum)  
0.35 to 0.65
%    
94.5 to 97.2
%    (estimate)
1.25 to 1.8
%    
0.2 to 0.55
%    
0.8 to 1.25
%    
0.01
%  (maximum)  
0.01
%  (maximum)  
0.2 to 0.6
%    
0.1
%  (maximum)  
0.05
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
610 to 700
MPa    
690
MPa  (minimum)  
16
% strain  (minimum)  
 