Chemical Composition
1.8
%  (maximum)  
0.15
%  (maximum)  
0.15
%  (maximum)  
92.9 to 98.5
%    (estimate)
0.5 to 1.75
%    
0.35
%  (maximum)  
1 to 2
%    
0.03
%  (maximum)  
0.03
%  (maximum)  
0.8
%  (maximum)  
0.05
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
400
MPa  (minimum)  
490 to 620
MPa    
20
% strain  (minimum)  
 
Other Information
Links