Chemical Composition
0.015 to 0.12
%    
0.18
%  (maximum)  
0.25
%  (maximum)  
96 to 99.8
%    (estimate)
1.7
%  (maximum)  
0.1
%  (maximum)  
0.01 to 0.06
%    
0.7
%  (maximum)  
0.035
%  (maximum)  
0.035
%  (maximum)  
0.15 to 0.5
%    
0.02 to 0.06
%    
0.02 to 0.2
%    
0.015 to 0.06
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
380
MPa    
520 to 680
MPa    
17 to 19
% strain    
 
Other Information
Links



No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®