Chemical Composition
0.02
%  (minimum)  
0.1
%  (maximum)  
0.3
%  (maximum)  
98.2 to 100
%    (estimate)
0.5
%  (maximum)  
0.03
%  (maximum)  
0.4
%  (maximum)  
0.025
%  (maximum)  
0.025
%  (maximum)  
0.4
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
260
MPa    
365 to 435
MPa    
27
% strain    
 
Other Information
Links