Chemical Composition
0.015
%  (minimum)  
0.13
%  (maximum)  
0.4 to 0.8
%    
0.25 to 0.55
%    
96.6 to 99.1
%    (estimate)
0.2 to 0.6
%    
0.15
%  (maximum)  
0.015 to 0.06
%    
0.65
%  (maximum)  
0.04
%  (maximum)  
0.035
%  (maximum)  
0.4
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
195
MPa    
22
% strain    
 
Other Information