Chemical Composition
0.15
%  (maximum)  
22 to 26
%    
54.9 to 67
%    (estimate)
2.5
%  (maximum)  
0.5
%  (maximum)  
11 to 15
%    
0.04
%  (maximum)  
0.03
%  (maximum)  
0.9
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
560
MPa  (minimum)  
26
% strain  (minimum)  
 
Other Information