Chemical Composition
0.15
%  (maximum)  
0.25
%  (maximum)  
97.3 to 99.8
%    (estimate)
1.6
%  (maximum)  
0.01 to 0.1
%    
0.03
%  (maximum)  
0.03
%  (maximum)  
0.15 to 0.5
%    
0.02 to 0.08
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
450
MPa    
550 to 720
MPa    
18
% strain    
 