Chemical Composition
2.6
%  (maximum)  
1 to 1.5
%    
60 to 70
%    (estimate)
1
%  (maximum)  
28 to 32
%    
0.08
%  (maximum)  
1 to 2.8
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
207
MPa  (minimum)  
379
MPa  (minimum)  
10
% strain  (minimum)  
131 to 193
   
 
Other Information