Chemical Composition
0.05 to 0.12
%    
0.9 to 1.4
%    
0.3
%  (maximum)  
94.8 to 98.2
%    (estimate)
0.4 to 1.5
%    
0.45 to 0.7
%    
0.01
%  (maximum)  
0.3
%  (maximum)  
0.03
%  (maximum)  
0.025
%  (maximum)  
0.8
%  (maximum)  
0.03
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
355
MPa  (minimum)  
510
MPa  (minimum)  
20
% strain  (minimum)  
 