Chemical Composition
0.05 to 0.15
%    
2 to 2.75
%    
0.5
%  (maximum)  
93.4 to 96.8
%    (estimate)
0.3 to 0.7
%    
0.9 to 1.2
%    
0.5
%  (maximum)  
0.04
%  (maximum)  
0.045
%  (maximum)  
0.6
%  (maximum)  
0.1
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
275
MPa  (minimum)  
485
MPa  (minimum)  
20
% strain  (minimum)  
201
 (maximum)  
 