Chemical Composition
0.07
%  (maximum)  
19 to 22
%    
3 to 4
%    
37.4 to 48.5
%    (estimate)
1.5
%  (maximum)  
2 to 3
%    
27.5 to 30.5
%    
0.04
%  (maximum)  
0.04
%  (maximum)  
1.5
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 