Range attributes
0.03
%  (maximum)  
20 to 22
%    
0.75
%  (maximum)  
41.3 to 50.3
%    (estimate)
2
%  (maximum)  
6 to 7
%    
0.18 to 0.26
%    
23.5 to 25.5
%    
0.04
%  (maximum)  
0.1
%  (maximum)  
1
%  (maximum)  
 
Discrete attributes
Short text attributes
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
USA
Corrosion resistant
CN3MN
ACI (SFSA)
 
Long text attributes
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Corrosion resistant
 