Chemical Composition
2.2 to 2.7
%    
0.2
%  (maximum)  
66 to 71.5
%    (estimate)
3.75 to 4.5
%    
21 to 24
%    
0.08
%  (maximum)  
1.5 to 2.5
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
172
MPa  (minimum)  
414
MPa  (minimum)  
25
% strain  (minimum)  
111 to 171
   
 
Other Information