Chemical Composition
0.24
%  (maximum)  
0.25
%  (maximum)  
0.35
%  (maximum)  
96.7 to 99.2
%    (estimate)
0.7 to 1.6
%    
0.08
%  (maximum)  
0.25
%  (maximum)  
0.035
%  (maximum)  
0.035
%  (maximum)  
0.15 to 0.5
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
Not Applicable
415
MPa  (minimum)  
550 to 690
MPa    
22
% strain  (minimum)  
 
Other Information