Chemical Composition
0.4 to 0.6
%    
0.65 to 0.95
%    
94.7 to 96.5
%    (estimate)
0.6 to 0.95
%    
0.2 to 0.45
%    
1.55 to 2
%    
0.025
%  (maximum)  
0.025
%  (maximum)  
0.15 to 0.35
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
448
MPa  (minimum)  
689
MPa  (minimum)  
14
% strain  (minimum)  
 
Other Information
Links



No warranty is given for the accuracy of these data