Chemical Composition
0.45 to 0.6
%    
0.8 to 1.15
%    
96.3 to 97.9
%    (estimate)
0.55 to 1.05
%    
0.15 to 0.5
%    
0.025
%  (maximum)  
0.025
%  (maximum)  
0.15 to 0.35
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
448
MPa  (minimum)  
689
MPa  (minimum)  
14
% strain  (minimum)  
 
Other Information
Links