Chemical Composition
0.45
%  (maximum)  
0.5 to 1.25
%    
93.4 to 96.9
%    (estimate)
0.6 to 1
%    
0.2
%  (minimum)  
1.65 to 3.5
%    
0.012
%  (maximum)  
0.015
%  (maximum)  
0.15 to 0.35
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
860
MPa  (minimum)  
18
% strain  (minimum)  
255 to 302
   
 
Other Information