Chemical Composition
0.31 to 0.65
%    
99.3 to 99.7
%    (estimate)
0.045
%  (maximum)  
0.045
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
1100
MPa  (minimum)  
1220
MPa  (minimum)  
8
% strain  (minimum)  
38 to 44
   
 