Chemical Composition
0.2 to 0.25
%    
0.45 to 0.65
%    
0.2 to 0.4
%    
96.7 to 97.9
%    (estimate)
0.9 to 1.2
%    
0.2 to 0.4
%    
0.04
%  (maximum)  
0.04
%  (maximum)  
0.15 to 0.35
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
940
MPa  (minimum)  
1040
MPa  (minimum)  
9
% strain  (minimum)  
33 to 39
   
 
Other Information
Links