Chemical Composition
0.035
%  (maximum)  
22 to 24
%    
0.4
%  (maximum)  
43.4 to 51.8
%    (estimate)
2
%  (maximum)  
6 to 6.8
%    
0.21 to 0.32
%    
20 to 22
%    
0.035
%  (maximum)  
0.02
%  (maximum)  
1
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 