Chemical Composition
0.95 to 1.05
%    
4.75 to 5.5
%    
89.2 to 93.2
%    (estimate)
0.75
%  (maximum)  
0.9 to 1.4
%    
0.03
%  (maximum)  
0.03
%  (maximum)  
1.5
%  (maximum)  
0.2 to 0.5
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 