Chemical Composition
0.42 to 0.5
%    
98.2 to 99
%    (estimate)
0.5 to 0.8
%    
0.035
%  (maximum)  
0.02 to 0.04
%    
0.1 to 0.4
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
275
MPa  (minimum)  
560
MPa  (minimum)  
14
% strain  (minimum)  
207
 (maximum)  
 
Other Information