Chemical Composition
0.37 to 0.44
%    
0.4
%  (maximum)  
97.4 to 99.1
%    (estimate)
0.5 to 0.8
%    
0.1
%  (maximum)  
0.4
%  (maximum)  
0.035
%  (maximum)  
0.02 to 0.04
%    
0.4
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
350
MPa  (minimum)  
600 to 780
MPa    
18
% strain  (minimum)  
 