Chemical Composition
0.12 to 0.18
%    
1.1 to 1.4
%    
92.8 to 94.4
%    (estimate)
0.25 to 0.55
%    
0.2 to 0.3
%    
3.8 to 4.3
%    
0.035
%  (maximum)  
0.035
%  (maximum)  
0.17 to 0.37
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
785
MPa    
1180 to 1470
MPa    
8
% strain    
 
Other Information