Chemical Composition
0.14 to 0.2
%    
0.8 to 1.1
%    
95.5 to 97.1
%    (estimate)
0.6 to 0.9
%    
0.15 to 0.25
%    
1.2 to 1.6
%    
0.035
%  (maximum)  
0.02 to 0.035
%    
0.4
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
740
MPa    
1100 to 1450
MPa    
8
% strain    
 
Other Information