Chemical Composition
0.14 to 0.2
%    
1.4 to 1.7
%    
95.3 to 96.7
%    (estimate)
0.3 to 0.6
%    
1.4 to 1.7
%    
0.035
%  (maximum)  
0.02 to 0.035
%    
0.4
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
590
MPa    
800 to 1100
MPa    
10
% strain    
 