Chemical Composition
0.58 to 0.65
%    
97.4 to 98.6
%    (estimate)
0.6 to 0.9
%    
0.08
%  (maximum)  
0.3
%  (maximum)  
0.04
%  (maximum)  
0.04
%  (maximum)  
0.2 to 0.5
%    
0.05
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
920 to 1050
MPa    
12
% strain    
 