Chemical Composition
0.54 to 0.6
%    
97.6 to 98.8
%    (estimate)
0.5 to 0.8
%    
0.08
%  (maximum)  
0.3
%  (maximum)  
0.04
%  (maximum)  
0.04
%  (maximum)  
0.2 to 0.5
%    
0.05
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
800 to 920
MPa    
14
% strain    
 
Other Information
Links



No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®