Chemical Composition
0.15
%  (maximum)  
0.4
%  (maximum)  
0.5
%  (maximum)  
93.2 to 96.5
%    (estimate)
0.5 to 0.8
%    
0.25
%  (maximum)  
3 to 4
%    
0.025
%  (maximum)  
0.025
%  (maximum)  
0.6
%  (maximum)  
0.03
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
275
MPa  (minimum)  
485
MPa  (minimum)  
24
% strain  (minimum)  
 
Other Information