Chemical Composition
0.4 to 0.48
%    
0.25
%  (maximum)  
97.1 to 98
%    (estimate)
1.35 to 1.65
%    
0.04
%  (maximum)  
0.24 to 0.35
%    
0.15
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
440
MPa  (minimum)  
640
MPa  (minimum)  
6
% strain  (minimum)  
229 to 269
   
 
Other Information