Chemical Composition
0.34 to 0.4
%    
0.8 to 1.1
%    
0.3
%  (maximum)  
96.3 to 97.9
%    (estimate)
0.6 to 0.9
%    
0.15 to 0.25
%    
0.3
%  (maximum)  
0.035
%  (maximum)  
0.03
%  (maximum)  
0.17 to 0.37
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
785
MPa  (minimum)  
930
MPa  (minimum)  
11
% strain  (minimum)  
241 to 269
   
 
Other Information